Researchers used a diamond-tipped nanoindenter on single-crystal molybdenum at room temperature. The PNAS paper reports that new, differently oriented grains formed after the probe made a sudden jump called a pop-in.

The team had to stop the indentation immediately after that first movement to observe the new grains. Continuing to press erased them, so the change was brief and confined to a tiny region around the indentation.

The study offers a way to observe transient changes in the metal's internal structure. It is a laboratory finding, not a demonstration of repairing a metal part or improving a working component.